Conference paper
Trigate 6T SRAM scaling to 0.06 μm2
M. Guillorn, J. Chang, et al.
IEDM 2009
A study was performed on the effect of liner thickness on electromigration lifetime. The measurement of electromigration lifetime, as a function of liner thickness for Cu/SiO2 interconnect structures was performed. Results showed a significant increase in mean lifetime for structures in which the liner thickness at the base of the test via was less than approximately 6 nm, with a current density<5mA/μm2 in the power line connected to the test via.